==Fiber Measurements==
==Fiber Measurements==
−
The paint thickness on the fibers should be between 10 and 20 microns.
+
The paint thickness on the fibers should be between 10 and 20 microns. It takes practice to achieve a consistently good layer, as the measurements from several tests show.
−
*[https://docs.google.com/file/d/0B4wCyytpeOAgdG5ubWpCc01OdVE/edit?usp=sharing Spreadsheet With Fiber Painting Measurements: Each test is on a separate sheet.]
+
+
*[https://docs.google.com/file/d/0B4wCyytpeOAgdG5ubWpCc01OdVE/edit?usp=sharing Spreadsheet With Fiber Painting Measurements]