When the light guides were placed in  heated ethanol concentrations, damage occurred to the fibers' cladding. Because it was significant damage, many concentrations were tested.  
 
When the light guides were placed in  heated ethanol concentrations, damage occurred to the fibers' cladding. Because it was significant damage, many concentrations were tested.  
   −
The procedure for the heated alcohol tests can be found [[Alcohol Test Procedure|here.]]
+
The procedure for the heated alcohol tests can be found [[https://docs.google.com/a/uconn.edu/document/d/1yUTqVM172Ta29nQGRo3gLhZzoSG-CtZQL-JCNUg0j8k|here.]]
     