Line 18: Line 18:     
Later we asked Dr. Jones about the flaring and he did not think it was a problem the way it was happening. If the the cladding is peeled back for more than 1 mm along the fiber, it is a problem, but that was not our situation. I went ahead with polishing bundle 407 and bottomed it out to 0.016".
 
Later we asked Dr. Jones about the flaring and he did not think it was a problem the way it was happening. If the the cladding is peeled back for more than 1 mm along the fiber, it is a problem, but that was not our situation. I went ahead with polishing bundle 407 and bottomed it out to 0.016".
 +
 +
1/11: Micah showed me how to remove excess material from the collars and bundling tools that were printed recently. I did that and sanded them in the morning. I polished a bundle of sci-fis with 1000 grit paper.